Spark plasma sintering of gas atomized Al 87 Ni 8 La 5 amorphous powder (original) (raw)

2009, Journal of Physics: Conference Series

Bulk samples were prepared by in-situ devitrification and consolidation of gas atomized Al 87 Ni 8 La 5 amorphous powder. Consolidation was carried out at different temperatures by spark plasma sintering, which leads to highly dense bulk specimens with a microstructure consisting of fcc aluminum together with Al 11 La 3 and Al 3 Ni intermetallic compounds. The consolidated powder displays a remarkably high compression stress, which depends on the sintering temperature and ranges between 900 and 1000 MPa, combined with plastic strain varying between 10 and 20 %. These results indicate that the mechanical properties of the samples can be tuned within a wide range of strength and ductility as a function of the sintering temperature used.

Sign up for access to the world's latest research.

checkGet notified about relevant papers

checkSave papers to use in your research

checkJoin the discussion with peers

checkTrack your impact

Loading...

Loading Preview

Sorry, preview is currently unavailable. You can download the paper by clicking the button above.